Freshly dried IL was charged with the solution of respective monomer and initiator—2,2′-azobisisobutyronitrile (0.1 wt% for AN; 0.5 wt% for MMA). The mass ratio between the monomer and the IL was 1:1.
Airplane wings and wind turbine blades are typically created using bulk polymerization in composite manufacturing facilities. They are heated and cured in enormous autoclaves and heated molds as big ...